Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1fU
SYNTHOS Krasten® 152 General Purpose Polystyrene
Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Styrolution Novodur® BX13036 ABS + PMMA
Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -20.0 °C
12.4 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -40.0 °C
12.4 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1fU
SYNTHOS Krasten® 172 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS..
Charpy Impact Unnotched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber
Reinforced with glass fiber and minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Charpy Impact Unnotched 2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
DIN 53453
Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber
Reinforced with glass fiber and minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Charpy Impact Unnotched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced
Radiflam® B is a range of flame retardant polybutylene terephthalate (PBT) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided ..