Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiflam® B is a range of flame retardant polybutylene terephthalate (PBT) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
Water Absorption 0.30 %
0.30 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
Elongation at Break 1.4 %
1.4 %
Tensile Modulus 10.1 GPa
1460 ksi
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
0.660 J/cm²

@Temperature 23.0 °C
3.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Comparative Tracking Index 250 V
250 V