Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid FGFTALX2-5 20 Polyamide 6, 25% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with glass fiber and minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.393 g/cc
0.05033 lb/in³
DIN 53479
Filler Content 23 - 27 %
23 - 27 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ISO 527-1,2
Elongation at Break 4.0 %
4.0 %
ISO 527-1,2
Tensile Modulus 2.90 GPa
421 ksi
ISO 527-1,2
Izod Impact, Notched (ISO) 3.50 kJ/m²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180
Charpy Impact Unnotched 2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
2.60 J/cm²

@Temperature -30.0 °C
12.4 ft-lb/in²

@Temperature -22.0 °F
DIN 53453
Charpy Impact, Notched 0.250 J/cm²

@Temperature -20.0 °C
1.19 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
0.280 J/cm²

@Temperature 23.0 °C
1.33 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 4.00 mm
V-2

@Thickness 0.157 in
MSZ 10383
Glow Wire Test 850 °C

@Thickness 1.50 mm
1560 °F

@Thickness 0.0591 in
IEC 685-2-1
960 °C

@Thickness 3.50 mm
1760 °F

@Thickness 0.138 in
IEC 685-2-1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 375 V
375 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714