Mechanical Properties Metric English Comments
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Akulon® K223-KM6 Nylon 6-30% Mineral Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179-1eU
Lanxess Durethan® A 30 H3.0 000000 Nylon 66
PA 66, non reinforced, injection molding, heat-ageing stabilized
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 757 G Q43 White 36609 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® HH-106 ABS
Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Terluran® HH-106 Q109 Colored ABS
Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic..
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2320 0035 LEV POM
Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF
Charpy Impact Unnotched 19.0 J/cm²

@Temperature -30.0 °C
90.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
Charpy Impact Unnotched 19.0 J/cm²

@Temperature 23.0 °C
90.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF