Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature 23.0 °C |
143 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature 23.0 °C |
143 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature -30.0 °C |
143 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® S3K Balance PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Charpy Impact Unnotched | 30.0 J/cm² @Temperature 23.0 °C |
143 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -20.0 °C |
>= 143 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature -40.0 °C |
>= 143 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Charpy Impact Unnotched | >= 30.0 J/cm² @Temperature 23.0 °C |
>= 143 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |