Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 51 T 60 PP, 60% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 60% microground, floated, chemically modified talc. General application in all industry. Delivered in natural mode and in t..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Charpy Impact Unnotched 0.700 - 1.20 J/cm²

@Temperature 23.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact Unnotched 0.700 - 1.10 J/cm²

@Temperature 23.0 °C
3.33 - 5.24 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Charpy Impact Unnotched 0.700 - 1.20 J/cm²

@Temperature 23.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²

@Temperature 23.0 °C
3.33 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)  (discontinued
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature -40.0 °C
3.33 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)  (discontinued
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)  (discontinued
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..