Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 0.900 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.500 - 0.900 J/cm²

@Temperature 23.0 °C
2.38 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Charpy Impact Unnotched 0.500 - 0.900 J/cm²

@Temperature 23.0 °C
2.38 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Charpy Impact Unnotched 0.700 - 0.900 J/cm²

@Temperature 23.0 °C
3.33 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eU
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Charpy Impact Unnotched 0.600 - 0.900 J/cm²

@Temperature 23.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..