Material Notes:
FeaturesModified homopolymer PP for injection moulding with the content of 60% microground, floated, chemically modified talc. General application in all industry. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 5.40 GPa
783 ksi
Flexural Strength 37.0 MPa
5370 psi
Flexural Modulus 5.00 GPa
725 ksi
Charpy Impact Unnotched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
0.150 J/cm²

@Temperature 23.0 °C
0.714 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Vicat Softening Point 160 °C
320 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi