Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 965 MPa | 140000 psi | Hard |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 965 MPa | 140000 psi | Stress relieved |