Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 963 MPa | 140000 psi | |
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
Tensile Strength at Break | 965 MPa | 140000 psi | Hard |
California Fine Wire Nickel 211 (Nickel Manganese Alloy) All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 965 MPa | 140000 psi | Stress relieved |
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |