Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 928 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.40 MPa
928 psi
Across flow; ASTM D412
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Tensile Strength at Break 6.40 MPa

@Time 7200 sec
928 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-1000 TPE
Product Description: StarFlex P 7380-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
Tensile Strength at Break 6.40 MPa
928 psi
ISO 37
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.40 MPa
928 psi
ISO 37
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.40 MPa
928 psi
ISO 37
Alliance Polymers Viprene™ G60A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G60A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 6.40 MPa
928 psi
ISO 37
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved