Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.40 MPa | 928 psi | Across flow; ASTM D412 |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Tensile Strength at Break | 6.40 MPa @Time 7200 sec |
928 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7380-1000 TPE Product Description: StarFlex P 7380-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tensile Strength at Break | 6.40 MPa | 928 psi | ISO 37 |
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.40 MPa | 928 psi | ISO 37 |
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.40 MPa | 928 psi | ISO 37 |
Alliance Polymers Viprene™ G60A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 6.40 MPa | 928 psi | ISO 37 |
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |