Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It has excellent physical properties, chemical resistance, and abrasion resistance.Applications: Protective coatingAbrasion resistant coatingPipe coatingFlooringRoof and deck coatingConstruction coatingIndustrial coatingLow cost moldsSpray-mold typeHighway and bridge overlaysWatertight coatingRoller, other casting elastomer replacementFoam surface protectionInformation provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
A component
1.10 g/cc
0.0397 lb/in³
B component
Viscosity 500 - 700 cP
500 - 700 cP
A component
1000 - 1200 cP
1000 - 1200 cP
B component
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 90
85 - 90
Tensile Strength at Break >= 7.85 MPa
>= 1140 psi
Elongation at Break >= 300 %
>= 300 %
Tear Strength >= 29.4 kN/m
>= 168 pli
Processing Properties Metric English Comments
Processing Temperature 60.0 - 65.0 °C
140 - 149 °F
Temperature setting, B component
65.0 - 70.0 °C
149 - 158 °F
Temperature setting, A component
Descriptive Properties Value Comments
Mixing Ratio 1:1