Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 407 MPa | 59000 psi | Stress relieved |
California Fine Wire Alloy 411 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |