Mechanical Properties Metric English Comments
Tensile Strength at Break 407 MPa
59000 psi
Stress relieved
California Fine Wire Alloy 411 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.