Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 51.0 - 53.0 MPa | 7400 - 7690 psi | DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Tensile Strength at Break | 46.0 - 53.0 MPa | 6670 - 7690 psi | 5 mm/min.; IS 867-1963 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |