Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 51.4 MPa | 7450 psi | ISO 527 |
Honeywell Aegis™ HFX High Barrier Nylon
(discontinued **) Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is .. |
|||
Tensile Strength at Break | 51.4 MPa | 7450 psi | ASTM D638 |
Styron Pulse® B-270 PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength at Break | 51.4 MPa | 7450 psi | ASTM D638 |
Entec Hyrene® PSCRY 2.5 General Purpose Polystyrene Available in North America Features: Crystal, General Purpose, and High Heat ResistanceRoHS Compliant Form: Pellets Information provided by Entec |