Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 - 0.018 cm/cm

@Thickness 3.17 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
Direction of Flow; ASTM D955
0.016 - 0.018 cm/cm

@Thickness 3.17 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
Transverse to Flow; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 70
60 - 70
ASTM D2240
Tensile Strength at Break 4.10 MPa
595 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Compression Set 30 %

@Temperature -5.00 °C,
Time 79200 sec
30 %

@Temperature 23.0 °F,
Time 22.0 hour
ASTM D395
Users viewing this material also viewed the following: