Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.6 - 38.6 MPa | 4000 - 5600 psi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |