Mechanical Properties Metric English Comments
Tensile Strength at Break 28.44 - 43.15 MPa
4125 - 6258 psi
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Tensile Strength at Break 28.44 - 42.17 MPa
4125 - 6116 psi
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Tensile Strength at Break 28.44 MPa
4125 psi
Taiwan PU Corporation TPU-EH90 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Tensile Strength at Break 28.44 MPa

@Temperature 100 °C,
Time 1.21e+6 sec
4125 psi

@Temperature 212 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
Seals Eastern 7344 Highly Saturated Nitrile Rubber