Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.4 MPa
3680 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of..
Tensile Strength at Break 25.4 MPa
3690 psi
ASTM D638
LyondellBasell Alathon® ETP H5057 High Density Polyethylene
ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit..
Tensile Strength at Break 25.4 MPa
3680 psi
ASTM D638
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon