Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® ETP H5057 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon® ETP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® ETP H5057 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavity stack molds, good color and organoleptic properties. Typical applications are rigid food containers such as cultured dairy product containers, margarine tubs, butter tubs, small frozen food containers and promotional drink cups.Regulatory StatusH 5057 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Processing TechniquesSpecific recommendations for processing H 5057 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Alathon® ETP (Enhanced Toughness and Processing), a Family of High Flow ResinsThis product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 57 g/10 min
57 g/10 min
ASTM D1238
Spiral Flow 53.8 cm
21.2 in
Measures the number on inches of flow produced when molten resin is injected into a long, spiral channel (0.625" insert), at a constant injection pressure of 1000 psi with a melt temperature of 440° F; Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 25.4 MPa
3690 psi
ASTM D638
Tensile Strength, Yield 21.4 MPa
3100 psi
Crosshead speed - 2"min.; ASTM D638
Elongation at Yield 9.5 %
9.5 %
Crosshead speed - 2" min; ASTM D638
1% Secant Modulus 979 MPa
142000 psi
Crosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 0.827 GPa
120 ksi
Crosshead speed - 0.5" min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 126 °C
259 °F
ASTM D1525