Tensile Strength at Break 25.4 MPa
3680 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of..
Tensile Strength at Break 25.4 MPa
3680 psi
ASTM D638
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon