Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1550 MPa | 225000 psi | Hard |
California Fine Wire Alloy 486 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire. |