Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 11.9 g/cc
0.430 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1450 MPa
210000 psi
Stress relieved
1550 MPa
225000 psi
Hard
Modulus of Elasticity 96.5 GPa
14000 ksi
Thermal Properties Metric English Comments
Melting Point 1700 °C
3092 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000101 ohm-cm
0.000101 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0001 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper +0.0028 mV