Mechanical Properties Metric English Comments
Tensile Strength at Break 1550 MPa
225000 psi
Hard
California Fine Wire Alloy 486 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.