Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.0 MPa | 2170 psi | Type IV Specimen; ASTM D638 |
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 818-073 offers the high environmental stress crack resistance characteristics of linear low density polyethylene with the processing properties needed for blowmolding and e.. |
|||
Tensile Strength at Break | 15.0 MPa | 2170 psi | ASTM D638 |
Teknor Apex APEX® 6500-85 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |