LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE GA 818-073 offers the high environmental stress crack resistance characteristics of linear low density polyethylene with the processing properties needed for blowmolding and extrusion applications. The broad molecular weight distribution of GA 818-073 combines good melt strength with a significantly reduced tendency to melt fracture, two drawbacks common to conventional fractional melt index LLDPE resins. Applications for this resin include beverage and drip irrigation tubing, squeeze tubes and bottles for pharmaceutical and personal care product packaging, drum liners, highway traffic channellizers and other large, blow molded parts.Processing TechniquesProcessing conditions can only be recommended when the type of equipment and end use applications are known. For further suggestions, please contact your Equistar sales representative. Regulatory StatusGA 818-073 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.9205 g/cc
0.03326 lb/in³
ASTM D1505
ESCR, Bottle >= 1000 hour
>= 1000 hour
ASTM D2561
Melt Flow 0.75 g/10 min
0.75 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength at Break 15.0 MPa
2170 psi
Type IV Specimen; ASTM D638
Elongation at Break >= 700 %
>= 700 %
Type IV Specimen; ASTM D638
Flexural Modulus 0.276 GPa
40.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °C
118 °F
ASTM D648
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Brittleness Temperature <= -42.0 °C
<= -43.6 °F
F<sub>50</sub>, Injection molded specimen; ASTM D746