Material Notes:
UV 422 is a semi-flexible, UV curing adhesive that can be used in a wide variety of potting, sealing, tacking and bonding applications. High strength bonds are formed to PVC and polycarbonate substrates and a wide variety of other substrates such as metals, epoxy-board, glass and other plastics in sealing and tacking applications. UV 422 forms shock absorbing bonds. Uses include flexible coatings and encapsulation.Applications: Transducer mountings, Switch potting, Connector sealing, Automotive components, Wire tacking.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Uncured
1.15 g/cc
1.15 g/cc
Of cured material
Water Absorption 0.43 %
0.43 %
Cured
Viscosity 3000 - 4000 cP

@Temperature 25.0 °C
3000 - 4000 cP

@Temperature 77.0 °F
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
Cured
Tensile Strength at Break 11.7 MPa
1700 psi
Cured
Elongation at Break 250 %
250 %
Cured
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
Cured
Maximum Service Temperature, Air 177 °C
351 °F
Cured
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Shrinkage 6.8 %
6.8 %
Upon cure, by volume
Descriptive Properties Value Comments
Color Clear/Light Straw Liquid
Composition Urethane Oligomer/ (Meth) Acrylate Monomer Blend
Solubility Alcohol, Chlorinated solvents
Toxicity Low