Mechanical Properties Metric English Comments
Tensile Strength at Break 168 MPa
24400 psi
50 mm/min; ASTM D638
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var..
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6
LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant.
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 (Asia Pacific)
LNP* Lubricomp* PFL-4216 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS
LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This ..
Tensile Strength at Break 168 MPa
24400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Strength at Break 168 MPa
24400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008ESZ PA 66
LNP* THERMOCOMP* RF008ESZ is a compound based on Nylon 6/6 containing 40% Glass Fiber. Added features of this grade include: Easy Molding, Heat Stabilized.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66
LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Strength at Break 168 MPa
24400 psi
ISO 527
SABIC Innovative Plastics LNP THERMOTUF RF008IS PA 66 (Asia Pacific)
LNP* Thermotuf* RF008IS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Strength at Break 168 MPa
24400 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 168 MPa
24400 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Strength at Break 168 MPa
24400 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Strength at Break 168 MPa
24400 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Strength at Break 168 MPa
24400 psi
ASTM D638
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant  (discontinued **)&l
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..