Polymer Property : Tensile Strength at Break = 1450 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1250 - 1450 MPa
181000 - 210000 psi
ThyssenKrupp SECURE 450 Structural Steel
This Material Specification applies to the liquid-quenched and tempered high-strength special steel SECURE 450 with a hardness between 400 - 480 HBW for civil use from 4 up to 20 mm thickness.Applic..
Tensile Strength at Break 1200 - 1450 MPa
174000 - 210000 psi
ThyssenKrupp SECURE MS special® Structural Steel
This Material Specification applies to the high-strength thermomechanically rolled special steel SECURE MS special® (ThyssenKrupp security steel for civil use) with a hardness from 350 to 450 HBW a..