Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF40-PEEK Polyetheretherketone, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetheretherketone with 40% long carbon fiber reinforcementInformation provided by P.. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific) LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 7.26 J/cm | 13.6 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Lubrilon® 646 Nylon 6/12, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |