PlastiComp Complet® LCF40-PEEK Polyetheretherketone, 40% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF40-PEEK Polyetheretherketone, 40% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetheretherketone with 40% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Filler Content 40 %
40 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 218 MPa
31600 psi
ASTM D-638
Elongation at Break 0.70 %
0.70 %
ASTM D-638
Tensile Modulus 37.89 GPa
5495 ksi
ASTM D-638
Flexural Strength 304 MPa
44100 psi
ASTM D-790
Flexural Modulus 25.386 GPa
3681.9 ksi
ASTM D-790
Izod Impact, Unnotched 7.26 J/cm
13.6 ft-lb/in
ASTM D-4812