Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.08 J/cm
13.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT
LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact.