Polymer Property : Izod Impact, Unnotched = 5.35 J/cm
Polymer Property :
Izod Impact, Unnotched =
5.35 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched
5.35
J/cm
10.0
ft-lb/in
ASTM D4812
SABIC Innovative Plastics REMEX VR4831 PBT
15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only