Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 17.88 J/cm | 33.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No.. |
|||
Izod Impact, Unnotched | 17.88 J/cm @Temperature 23.0 °C |
33.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Faradex DS0036IP PC LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
Izod Impact, Unnotched | 17.88 J/cm @Temperature 23.0 °C |
33.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific) LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |
|||
Izod Impact, Unnotched | 17.88 J/cm @Temperature 23.0 °C |
33.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East) LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B.. |