Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 13.1 J/cm | 24.5 ft-lb/in | ASTM D-4812 |
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 13.1 J/cm | 24.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare |
|||
Izod Impact, Unnotched | 13.1 J/cm | 24.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |