Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Velocity®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Filler Content 50 %
50 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 234 MPa
33900 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 16.21 GPa
2351 ksi
ASTM D-638
Flexural Strength 352 MPa
51100 psi
ASTM D-790
Flexural Modulus 13.79 GPa
2000 ksi
ASTM D-790
Izod Impact, Notched 2.94 J/cm
5.51 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 13.1 J/cm
24.5 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
ASTM D-648