Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.40 - 2.67 J/cm
4.50 - 5.00 ft-lb/in
Average value: 2.56 J/cm Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
Izod Impact, Unnotched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Average value: 2.21 J/cm Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..
Izod Impact, Unnotched 0.908 - 2.67 J/cm
1.70 - 5.00 ft-lb/in
Average value: 1.99 J/cm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..