Polymer Property : Izod Impact, Unnotched = 16.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.0 J/cm

@Temperature 23.0 °C
30.0 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D4812
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched 16.0 J/cm

@Temperature 23.0 °C
30.0 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D4812
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP)
PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop..
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene
DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene
DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive)
CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provid..
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war..
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene
DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene
DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene
DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman.
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D4812
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified
Information provided by Asahi Thermofil