Material Notes:
CN-SS is filled with small non-sloughing stainless steel fibers. Has high flexural strength and good thermal stability to 275F. The CN-SS material has excellent impact strength. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.13 %
0.13 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 16.0 J/cm
30.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
285 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.65 mm
V-0

@Thickness 0.0650 in
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Dry; ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B