Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.497 - 13.3 J/cm | 0.930 - 25.0 ft-lb/in | Average value: 6.94 J/cm Grade Count:7 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Unnotched | 1.44 - 13.3 J/cm | 2.70 - 25.0 ft-lb/in | Average value: 4.11 J/cm Grade Count:27 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched | 2.51 - 13.3 J/cm | 4.70 - 25.0 ft-lb/in | Average value: 4.72 J/cm Grade Count:12 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Unnotched | 3.74 - 13.3 J/cm | 7.00 - 25.0 ft-lb/in | Average value: 6.86 J/cm Grade Count:10 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Izod Impact, Unnotched | 1.17 - 13.3 J/cm | 2.20 - 25.0 ft-lb/in | Average value: 5.86 J/cm Grade Count:31 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 3.74 - 13.3 J/cm | 7.00 - 25.0 ft-lb/in | Average value: 7.85 J/cm Grade Count:74 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 1.33 - 13.3 J/cm | 2.50 - 25.0 ft-lb/in | Average value: 7.27 J/cm Grade Count:97 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 9.08 - 13.3 J/cm | 17.0 - 25.0 ft-lb/in | Average value: 10.7 J/cm Grade Count:5 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched | 2.67 - 13.3 J/cm | 5.00 - 25.0 ft-lb/in | Average value: 7.52 J/cm Grade Count:25 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 3.74 - 13.3 J/cm | 7.00 - 25.0 ft-lb/in | Average value: 7.98 J/cm Grade Count:54 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched | 2.40 - 13.3 J/cm | 4.50 - 25.0 ft-lb/in | Average value: 5.97 J/cm Grade Count:14 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |