Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.30 J/cm @Thickness 3.18 mm |
11.8 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer LNP LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing 25% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA (Asia Pacific) LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.32 J/cm @Temperature 23.0 °C |
11.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Unnotched | 6.32 J/cm | 11.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |
|||
Izod Impact, Unnotched | 6.30 J/cm | 11.8 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 633 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |