Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
50 mm/min; ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.30 J/cm
11.8 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 3.20 mm
194 °F

@Thickness 0.126 in
unannealed; ASTM D648