Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D4812
PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF30-PBT Polybutylene Terephthalate, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polybutylene Terephthalate (PBT) with 30% long glass fiber reinforcementInformation pr..
Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Izod Impact, Unnotched 11.75 J/cm

@Temperature 23.0 °C
22.01 ft-lb/in

@Temperature 73.4 °F
ASTM D4812
DuPont Performance Polymers Rynite® RE15022 NC010 PET  (Unverified Data**)
Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.