PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 238 MPa
34500 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 37.93 GPa
5501 ksi
ASTM D638
Flexural Strength 441 MPa
64000 psi
ASTM D790
Flexural Modulus 27.59 GPa
4002 ksi
ASTM D790
Izod Impact, Notched 2.94 J/cm
5.51 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.75 J/cm
22.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648