Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Izod Impact, Unnotched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Izod Impact, Unnotched | 0.880 J/cm - NB | 1.65 ft-lb/in - NB | Average value: 12.9 J/cm Grade Count:88 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Izod Impact, Unnotched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |