Mechanical Properties Metric English Comments
Creep Strength 60.0 MPa

@Strain 0.700 %,
Time 360000 sec
8700 psi

@Strain 0.700 %,
Time 100 hour
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Creep Strength 60.0 MPa

@Time 360 sec,
Strain 0.400 %
8700 psi

@Time 0.100 hour,
Strain 0.400 %
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Creep Strength 60.0 MPa

@Strain 0.500 %,
Time 3600 sec
8700 psi

@Strain 0.500 %,
Time 1.00 hour
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Creep Strength 60.0 MPa

@Strain 0.600 %,
Time 36000 sec
8700 psi

@Strain 0.600 %,
Time 10.0 hour
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Creep Strength 60.0 MPa

@Temperature 150 °C,
Time 720000 sec
8700 psi

@Temperature 302 °F,
Time 200 hour
0.5% strain
AMT AM-Lite® Die Casting Magnesium Alloy
AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has..