Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 60.0 MPa @Strain 0.700 %, Time 360000 sec |
8700 psi @Strain 0.700 %, Time 100 hour |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Creep Strength | 60.0 MPa @Time 360 sec, Strain 0.400 % |
8700 psi @Time 0.100 hour, Strain 0.400 % |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Creep Strength | 60.0 MPa @Strain 0.500 %, Time 3600 sec |
8700 psi @Strain 0.500 %, Time 1.00 hour |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Creep Strength | 60.0 MPa @Strain 0.600 %, Time 36000 sec |
8700 psi @Strain 0.600 %, Time 10.0 hour |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Creep Strength | 60.0 MPa @Temperature 150 °C, Time 720000 sec |
8700 psi @Temperature 302 °F, Time 200 hour |
0.5% strain |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |