Mechanical Properties Metric English Comments
Creep Strength 138 MPa

@Temperature 816 °C,
Time 3.60e+6 sec
20000 psi

@Temperature 1500 °F,
Time 1000 hour
0.5% Creep
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Creep Strength 138 MPa

@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi

@Temperature 1100 °F,
Time 10000 hour
1% creep
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Creep Strength 138 MPa

@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi

@Temperature 1100 °F,
Time 10000 hour
1% creep
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Creep Strength 138 MPa

@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi

@Temperature 1100 °F,
Time 10000 hour
1% creep
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Creep Strength 138 MPa

@Temperature 593 °C,
Time 3.60e+7 sec
20000 psi

@Temperature 1100 °F,
Time 10000 hour
1% creep
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..